Many of Micro Powders’ most successful products are based on our innovative Composite Technology, where two or more materials are mixed, extruded, and then micronized.
TEGO® Powder Aid D01 makes the formulation easier to disperse during extrusion by promoting pigment wetting, and effectively reducing melt viscosity. The lower melt viscosity also leads to better degassing, which aids flow and leveling as the formulation cures and prevents pinholes in the coating.