Recently, considerable development work has been conducted to demonstrate the enhanced performance and improved economics associated with new and novel white pigment offerings. This article highlights a newwhite pigment that is showing great promise at reducing the amount of titanium dioxide needed to formulate cool roof coatings while enhancing performance, processability, and affordability.