In conjunction with the Institute for Materials and Wood Technology at the Bern University of Applied Sciences, AVALON Industries is launching a research project to replace formaldehyde in phenol-formaldehyde (PF) resins with biobased, nontoxic platform chemical 5-HMF (5-hydroxymethylfurfural).