The American Architectural Manufacturers Association (AAMA) recently released an updated document describing the test procedures and performance requirements for pigmented organic coatings applied to aluminum, fiber reinforced thermoset or wood and cellulosic composite profiles for windows, doors, wall panels, skylights, sloped glazing and similar products.