PPG Announces Acquisition Agreements June 14, 2015 No Comments PPG Industries has reached a definitive agreement to acquire IVC Industrial Coatings Inc., a U.S.-based specialty powder and liquid coatings manufacturer with 2014 sales of more than $100 million. Read More