Business Unit of Flint Group Transfers Production of UV Inks April 8, 2015 No Comments Flint Group announced that in the second half of 2014, all production of UV inks was moved from Baranzate, Italy, to a new center of excellence in UV ink production in Trelleborg, Sweden. Read More