Pore-Free Graphene Oxide Film Promises Advancements in Protective Coatings September 19, 2024 No Comments A breakthrough film offers 100,000x better hydrogen ion barrier protection, setting new standards for advanced coatings. Read More
Freshmen-Level Chemistry Solves the Solubility Mystery of Graphene Oxide Films February 8, 2015 No Comments A Northwestern University-led team recently found the answer to a mysterious question that has puzzled the materials science community for years, and it came in the form of some surprisingly basic chemistry. Read More