Metal Ink Could Ease Way Toward Flexible Electronic Books and Displays January 19, 2014 No Comments Scientists are reporting the development of a novel metal ink made of small sheets of copper that can be used to write a functioning, flexible electric circuit on regular printer paper. Read More