PPG Electrocoat Primer Qualified to Aerospace Specification January 10, 2014 No Comments PPG Industries’ aerospace coatings group has qualified AEROCRON™ electrocoat primer to SAE International’s Aerospace Material Specification 3144 for anodic electrodeposition primer for aircraft applications. Read More