Hard and Invisible Nanosilica Particle Technology in Solventborne, High-Gloss, Two-Pack PUR Clearcoats for Plastics Marco Heuer Fabian Eichenberger Sascha Herrwerth January 6, 2014 No Comments Traditional two-pack PUR technology combined with surface-modified nanosilica particles results in increased scratch and abrasion resistance in transparent, high-gloss coatings for plastics.Read More