ASTM Developing Palladium-Cobalt Alloy Standard December 4, 2011 No Comments Increasing interest in the various uses of electrical contacts is the leading impetus for the development of a proposed new standard, ASTM WK34423, Specification for Electrodeposited Coatings of Palladium-Cobalt Alloy for Engineering Use. Read More