Time to Reconsider the Color Red for Underwater Hulls Poseidon Sciences Group November 22, 2024 2 Comments Barnacles prefer red hulls, disrupting tradition. New research suggests lighter colors like white could enhance marine coatings’ performance and sustainability.Read More