As the TiO2 market strengthens post-pandemic, TiO2 consumers in North America will continue to be faced with the dilemma of how best to find reductions in TiO2 costs.
Customers can now order less than a single box (in quantities as little as 0.9 kg) of selected Interpon Ready-to-Ship powders (there are nearly 500 to choose from) and have them shipped within three business days or faster.
When the Florida Roofing & Sheet Metal Contractors Association (FRSA) designed its new headquarters, they knew it needed to be built with materials that were energy-efficient, code-compliant and long lasting. To ensure a long-lasting exterior, they turned to coatings and component finishes made with Kynar 500 and Kynar Aquatec PVDF resin.
The average molecular weight of a latex can be influenced by a number of factors, but it is often not realized that the number of particles in the latex (which is directly related to particle size) is important in determining molecular weight.
In the development of a low- VOC, self-healing epoxy hybrid primer, this company leveraged its self-healing technology to design a waterborne protective primer with an unprecedented combination of corrosion resistance and eco-friendliness.
NanoRustX (NRX) NanoPrime works by chemically reacting with iron and iron oxide (rust) to form iron phosphate and creates a nano bond with both metallic and painted surfaces. The chemically bonded layer is insoluble and extremely corrosion resistant.
This work deals with the assessment of fungal deterioration on different anti-corrosive coatings using electrochemical techniques (corrosion potential and ionic resistance).
Automotive companies and coaters recognize the need to monitor viscosity, but making that measurement outside the laboratory has challenged process engineers and quality departments. Automated in-line viscosity measurement enables continuous monitoring of paint at the point of application.