CPS Color Group Oy has acquired Switzerland-based Pinova AG. Pinova is a market leader in colorants for facade coatings and wet plasters in German-speaking Europe and Central and Eastern Europe countries.
At Tuesday morning’s session at CTT, Tom Quantrille, Advanced Composite Materials, LLC, presented a paper on the use of silicon carbide single crystals, also known as “whiskers”, for use
Dr. Richard D. Jenkins, Global Group President, Arkema Coating Resins, delivered this morning’s keynote address at the 2011 Coatings Trends & Technologies conference in Oak Brook, IL. His presentation,
The RPM Wood Finishes Group, a leading manufacturer of wood coatings and touch-up and repair products, has acquired Fuhr Industrial, a provider of waterborne wood coating products and technologies based in Mansfield, TX.
Clariant has adjusted its guidance for the full-year 2011 due to unfavorable foreign exchange rate developments and a softening of the global economy in the current business year.