PPG Industries’ industrial coatings business has created a dedicated electronic materials group to integrate products and technologies acquired from Spraylat Corp., Mt. Vernon, NY.
Heraeus Noblelight, a business group of the Hanau, Germany-based precious metal and technology group Heraeus, has successfully completed the acquisition of the Fusion UV Systems Group, headquartered in Gaithersburg, MD.
Paint and coating additives manufacturer Dover Chemical Corp. has made a series of leadership changes designed to prepare the company for future growth.
Global alternative asset manager The Carlyle Group L.P. has completed its acquisition of paint and coatings manufacturer DuPont Performance Coatings for $4.9 billion.
A new ASTM International standard describes methods of preparing surfaces of hot-dip galvanized iron and steel for powder coating and the application of powder coating materials.