Aqueous fumed silica dispersions are a new form
of a well-known, long-standing additive that can improve a variety of
performance attributes in waterborne coatings.
This article examines the parameters of
wavelength, peak irradiance and energy density that comprise UV curing as well
and some common issues related to measuring them.
To save automakers and automotive suppliers
considerable time and money in applying metallic flake and other effect paints, X-Rite launched its xDNA®
system with the MA98® handheld spectrophotometer.
Atlas Material Testing Technology developed the
Right Light™ filter, which used with a xenon light source, simulates
environmental conditions at an accelerated rate.