Dow Coating Materials (DCM), a global business unit of The Dow Chemical Company, announces a new addition to its product line of APEO-free surfactants.
Pull-off adhesion testing was carried out to determine the adhesion of a solvent-free, two-component epoxy coating to a substrate when applied by plural airless spray and by hand.
A unique acrylic/polyurethane technology has been described that offers a new mechanism for the faster release of coalescent from industrial wood coatings.
A new type of ceramic coating now on the market is not only completely VOC-free, but is also promising to deliver an abrasion-, corrosion-, high-temperature- and chemical-resistant finish that can be applied in a high build, single coat with no primer by a licensed contractor.
To reduce the VOCs used in PU-based coatings, Yantai Wanhua Polyurethanes Co. Ltd. developed waterborne technologies including PUD, PUA and waterborne 2K.