PITTSBURGH  – Steelscape is now offering metallic-coated and pre-painted steel with DURANAR® GR (graffiti-resistant) and CORAFLON® GR coatings from PPG Industries’ building products group.

Duranar GR and Coraflon GR three-coat systems feature a primer and color coat topped with a graffiti-resistant clearcoat that can be cleaned with DURAPREP® Prep 400 graffiti remover by PPG. If the Steelscape steel is spray-painted, graffiti can be eliminated by applying the graffiti remover directly to the stain, allowing it to sit for 10 to 60 seconds, then wiping it with a clean cloth or scrubbing it with a nylon brush. Most stains can be removed in 10 minutes or less.

When applied on either Duranar GR or Coraflon GR clear coatings, Duraprep Prep 400 field-applied graffiti remover also can eradicate paint overspray, pen and marker ink, lipstick, scuff marks, tape residue, bugs, tar and many other substances that mar the appearance of steel building panels.