www.pcimag.com/articles/99866-a-coating-that-protects-against-heat-and-oxidation
Industrial Coatings

A Coating That Protects Against Heat and Oxidation

November 16, 2014

MUNICH, Germany - Researchers have developed a coating technique that they plan to use to protect turbine engine and waste incinerator components against heat and oxidation. A topcoat from micro-scaled hollow aluminum oxide spheres provides heat insulation, in the lab, already proved more economical than conventional techniques.

Gases don’t conduct heat as well as solids do. Cellular or aerated concretes take advantage of this effect, which experts call “gas-phase insulation.” The heat barrier is achieved by air encased in the cavities of the concrete. But gas-phase insulation has far greater potential than keeping our homes warm. It can also be used to protect turbine engine and waste incinerator components when subjected to intense heat. All that is needed is to transfer this effect to a coating that is just a few hundred micrometers thick.

Temperature Differences of Over 400 °C

Scientists at the Fraunhofer Institute for Chemical Technology ICT in Pfinztal have not only done just that, they’ve also done it in a particularly economical way. They’ve designed a coating that consists of an outer topcoat from conjoined aluminium oxide spheres. “These spheres are hollow and filled with gas,” explains coatings expert Dr. Vladislav Kolarik from the ICT’s Energetic Systems department. When the outer side of a part is exposed to temperatures of 1000 °C, these gas-filled spheres reduce temperatures on the part’s inner side to under 600 °C – as the ICT scientists have demonstrated in their laboratories. Since gas and steam turbines used for energy generation, combustion chambers, waste incinerator generators and temperature sensors, and reactors in the chemical and petrochemical industries are all subjected to temperatures of up to 1000 °C, there is considerable demand of thermal protection.

What’s most remarkable is that the heat-insulating layer from hollow aluminum oxide spheres is obtained on the basis of a conventional, economic process. Operators only have to do some simple math to see the benefits: conventional thermal barrier techniques – most of which are based on ceramic materials – are expensive. The process the scientists adapted was originally designed to protect metallic components from oxidation. “We’ve optimized the technique so that the coat not only retains its oxidation protection, but furthermore protects against heat,” says Dr. Kolarik. The basic coating layer forms by interaction of aluminum particles and the metallic component. This is done by depositing aluminum powder on the surface of the metal and heating it all up to a suitable temperature over several hours. The result is an aluminum-rich coating on the component’s surface that protects against oxidation at high temperature. With the new procedure, the topcoat from the hollow aluminum oxide spheres is additionally formed. “Up to now, it never occurred to anyone to use these spheres to produce another coating layer – they were just a waste product,” says Dr. Kolarik.

Now the scientists have refined the process so they can produce both coating layers in the required thickness. The way it works is to take aluminum particles and mix them with a viscous liquid bonding agent. This produces a substance similar to a paint or slurry, which the scientists then manually paint, spray or brush onto the metallic component. “All that’s left is to add a fair bit of heat,” says Dr. Kolarik. But it’s all easier said than done: Dr. Kolarik and his team have had to precisely fine tune the size and size distribution of the aluminum particles, the temperature and duration of the heating stage, and the viscosity of bonding agents. “Just like a master chef, the first job was to come up with a winning recipe.”

“We’re currently in the process of putting the findings from the EU-funded PARTICOAT project into practice. This involves coating bigger and bigger components without exceeding the temperature limits for each application area. At the same time we’re trying out techniques to automate the whole coating process. Our plan is to follow in the footsteps of the aerated concrete that helps insulate our homes – that’s been in series production for a long time now,” says Dr. Kolarik.