Intumescent Coating
August 20, 2014
With protection for up to 60 minutes, the unique features of FIRETEX FX5062 mean greater design flexibility and lower loadings are now possible across a diverse range of steel sections.
Developed for on-site application, the water-based thin-film intumescent coating can be applied as a high-build single coat. It is designed for use in dry controlled environments without top coats - meeting the requirements of ISO 12944-2: 2007 - and semi-controlled environments with a top coat to ISO 12944-2: 2007.
Accreditations include Certifire and the recently revised ASFP Yellow Book Rev 5, including the fire testing protocol for cellular beam protection. Application can be through standard airless spray equipment including petrol-powered pumps.