This super-slippery, permanently wet coating prevents paint products from sticking to cans and manufacturing equipment, reducing waste. It improves energy efficiency and reduces paint build-up on equipment. It was tested with more than 30 unique paint formulations and colors, including water-based paints and colorants on coated high-density polyethylene surfaces. E-mail info@liquiglide.com.