Surface Analyzer

KRÜSS

June 1, 2014

 The Mobile Surface Analyzer measures wettability based on the contact angle using two test liquids simultaneously. Fully automated and using the innovative “One-Click SFE” method, it provides values for the two contact angles, the surface-free energy of the sample and its polar part. The simultaneous dosing and analysis of two drops eliminate the need to change the test liquid during the material testing. Visit www.kruss.de