www.pcimag.com/articles/99025-fillers-extenders-oils-and-lubricants-on-display-at-re-carrolls-booth

Fillers, Extenders, Oils and Lubricants on Display at R.E. Carroll’s Booth
April 10, 2014
R.E. Carroll is exhibiting fillers, extenders, oils and lubricants at Booth 222. For over 88 years, the company has been supplying the industry with raw materials and service. Its expanding raw material product line features OCI fumed silica, GPR calcium carbonates from Kinsley Materials, Novacite ground silica from Malvern Minerals, and hydrocarbon resins from Rezchem. Also included are coalescing agents and non-phthalate plasticizers from American eChem; cellulose ethers, organo clay and redispersable polymer powders from Yil-Long; and many other products.