To complement the existing Tefzel® products, an expanded product line features a powder primer (532-6405) and a new high-build clear topcoat (532-6410). The new high-build product can be applied to film builds of 80-100 mils, depending on part geometry. Tefzel is a rugged thermoplastic with an outstanding balance of properties. When compared against the competition, it provides several thermal advantages, such as better chemical resistance at higher operating temperatures, a higher melting point that provides improved thermal stability, and lessened low-temperature embrittlement. In addition to these qualities, Tefzel is extremely tough and electrically insulative with superior substrate adhesion. Its characteristics make the coating an ideal candidate in markets such as chemical processing, semiconductor, pharmaceutical and food processing.