NEWS

Nubiola Increases Production Capacity

February 16, 2014

BARCELONA, Spain - Nubiola announced that it is increasing its production capacity of zinc ferrites, Nubifer K Series, by approximately 33 percent. Full implementation of the capacity expansion is expected by the last quarter of 2014.

The company’s Nubifer K Series are beige, tan color complex organic pigments with a ZnFe2O4 spinel crystal structure that withstand high temperatures and provide excellent light, weather and chemical fastness with a high dimensional stability in polyolefins, hiding power and opacity.