Sherwin-Williams Protective and Marine Coatings

July 3, 2013

Magnalux 404 FF styrene-free vinyl ester is designed for use with steel and concrete substrates in the oil and gas market. The new coating is specially formulated to combat immersion and containment service corrosion caused by contact with aggressive chemicals such as aromatic solvents, high-aromatic gasoline, ethanol gasohol, MTBE, ETBE, TAME and ether/fuel blends.