Diacetanil Orange HP 3428C (PO34) and Carmine HP 7638C (PR176) high-purity pigments are suitable for ink applications where a high chemical purity is required, such as food packaging and personal care products. These grades are introduced to guarantee a specific chemical purity and reduce migration risk, minimizing the risks for carcinogenic, mutagenic and skin irritation effects. E-mail info@cappelle.be.