www.pcimag.com/articles/96658-pigments

Pigments
July 2, 2012
Nubifer Y-7050 is a new heat-resistant yellow iron oxide that is created to withstand high temperatures when processing. Together with the company’s Nubifer K series Zinc Ferrites, it forms a heat-resistant beige pigment range. Visit www.nubiola.com.