www.pcimag.com/articles/95887-scs-plans-new-coating-center-in-texas

SCS Plans New Coating Center in Texas

January 4, 2012
INDIANAPOLIS – Specialty Coating Systems (SCS) announced the expansion of its Parylene coating service operations into the southern United States. Build-out is underway for a new 13,000-square-foot facility located in Austin, TX. The new coating center will begin full production operations in early 2012.