www.pcimag.com/articles/95755-overspray-collection-media-captures-carcs-posted-6-17-08

Overspray Collection Media Captures CARCs - Posted 6/17/08

June 17, 2008

CARC (chemical agent resistant coating) overspray collection media from Columbus Industries is designed to provide an extended filter service life and high particulate removal efficiency when using CARC systems. The combination baffle/strainer-type construction consists of layers of slit and expanded kraft with a final layer of synthetic polyester backing to maximize efficiency and strength. Layers are arranged in a graduated density pattern to redirect and cause the particulate-laden airflow to become turbulent, resulting in maximum contact between the overspray and the baffles within the collectors.

For more information, call 740.983.2552 or visit www.colind.com.