Dynamix Black 30C933 from The Shepherd Color Co. is a “stir-in” inorganic color pigment (CI Pigment Black 26) that can be used in liquid and powder coatings, silicate and masonry coatings, and radiation-cured coatings.

Dynamix Black 30C933 from The Shepherd Color Co. is a “stir-in” inorganic color pigment (CI Pigment Black 26) that can be used in liquid and powder coatings, silicate and masonry coatings, and radiation-cured coatings. The pigments require only simple mixing. Complete dispersion can be achieved in as little as 5 minutes, depending on the intensity of the mixing equipment. The pigments are compatible with solvent-based and waterborne coatings systems, as well as 100% solids systems and UV-cured coatings.