www.pcimag.com/articles/95469-materials-new-coating-protects-against-ballistic-fragments-posted-2-6-08
MATERIALS: New Coating Protects Against Ballistic Fragments - Posted 2/6/08
February 6, 2008
PAXCON PX-2100 from LINE-X® Franchise Development Corp. is a high-performance chemical formulation developed to protect against spalling and fragmentation during a ballistic attack.
PAXCON PX-2100 from LINE-X® Franchise Development Corp. is a high-performance chemical formulation developed to protect against spalling and fragmentation during a ballistic attack. The product encapsulates bullets and other ballistic objects, which will remain intact and pose no secondary damage. The coating can be sprayed over any surface hard enough to cause a projectile to spall, such as aluminum, ceramic or steel.
In 2007, the product was certified by H.P. White Laboratory, Inc., one of the oldest and most respected ballistic and research centers in the nation. Ity was also selected for anti-spalling protection by MRAP (Mine Resistant Ambush Protected) vehicle manufacturers, the Pentagon's top military personnel protection initiative.
For specific results from the H.P. White certification, contact Steve Decker at 301.862.7717 or steve@LineXcorp.com. For more information about the coating, visit www.PAXCON.com.
PAXCON PX-2100 from LINE-X® Franchise Development Corp. is a high-performance chemical formulation developed to protect against spalling and fragmentation during a ballistic attack. The product encapsulates bullets and other ballistic objects, which will remain intact and pose no secondary damage. The coating can be sprayed over any surface hard enough to cause a projectile to spall, such as aluminum, ceramic or steel.
In 2007, the product was certified by H.P. White Laboratory, Inc., one of the oldest and most respected ballistic and research centers in the nation. Ity was also selected for anti-spalling protection by MRAP (Mine Resistant Ambush Protected) vehicle manufacturers, the Pentagon's top military personnel protection initiative.
For specific results from the H.P. White certification, contact Steve Decker at 301.862.7717 or steve@LineXcorp.com. For more information about the coating, visit www.PAXCON.com.