www.pcimag.com/articles/95457-materials-enviro-friendly-stripper-removes-permanent-paints-posted-2-6-08
MATERIALS: Enviro-Friendly Stripper Removes "Permanent" Paints - Posted 2/6/08
February 6, 2008

ACL-707 Green Piranha from Applied Chemical Laboratories, Inc. is a high-performance, environmentally friendly stripper for removing otherwise permanent paints from metallic surfaces. According to the company, the new formulation quickly and easily strips polymer coatings such as epoxy, polyester, urethane, TGIC and hybrid powders; as well as military epoxies, high and low baked water, Teflon, Xylan, Halar and other liquid and dry industrial coatings. The product is 100% compatible for use with sensitive alloys including aluminum and magnesium. Tenacious coatings are quickly removed without damaging the substrate or changing critical dimensions or tolerances.
Proprietary, corrosion inhibiting technology prevents damage to traditional surface preparations such as anodized aluminum, chrome, nickel, zinc and other plating. Even mirror polished aluminum and other cosmetic surface treatments remain damage free. The product is available in 5 and 55 gallon containers, and 330 gallon totes (IBCs).
For more information, visit www.appchem.com.