A team of Northwestern University researchers has developed a new anode coating strategy that significantly enhances the efficiency of solar energy power conversion. The technology uses a laser deposition technique that coats the anode of a plastic bulk-heterojunction cell with a very thin (5 to 10 nanometers thick) and smooth layer of nickel oxide.

A team of Northwestern University researchers has developed a new anode coating strategy that significantly enhances the efficiency of solar energy power conversion. Tobin J. Marks, the Vladimir N. Ipatieff Research Professor in Chemistry in the Weinberg College of Arts and Sciences and professor of materials science and engineering, and Robert Chang, professor of materials science and engineering in the McCormick School of Engineering and Applied Science, led the research team. Other Northwestern team members were researcher Bruce Buchholz and graduate students Michael D. Irwin and Alexander W. Hains.

The Northwestern researchers employed a laser deposition technique that coats the anode of a plastic bulk-heterojunction cell with a very thin (5 to 10 nanometers thick) and smooth layer of nickel oxide. This material is an excellent conductor for extracting holes from the irradiated cell but, equally important, is an efficient “blocker” which prevents misdirected electrons from straying to the “wrong” electrode (the anode), which would compromise the cell energy conversion efficiency.

In contrast to earlier approaches for anode coating, the Northwestern nickel oxide coating is cheap, electrically homogeneous and non-corrosive. In the case of model bulk-heterojunction cells, the Northwestern team has increased the cell voltage by approximately 40% and the power conversion efficiency from approximately 3 to 4% to 5.2 to 5.6%.

The researchers currently are working on further tuning the anode coating technique for increased hole extraction and electron blocking efficiency and moving to production-scaling experiments on flexible substrates.