PPG Aerospace, Altairnano Developing Chromate-Free Aircraft Primer - Posted 9/19/07
September 19, 2007
PPG Industries’ aerospace business and Altair Nanotechnologies have agreed to jointly develop and commercialize environmentally friendly nanoparticle technology to replace chromate in an aircraft primer that affords excellent corrosion resistance in high-solids and waterborne formulas.
PPG Industries’ aerospace business and Altair Nanotechnologies have agreed to jointly develop and commercialize environmentally friendly nanoparticle technology to replace chromate in an aircraft primer that affords excellent corrosion resistance in high-solids and waterborne formulas. Terms were not disclosed.
The companies will develop a nanometal oxide dispersion technology under a three-year research agreement, with an added five-year contract for commercialization and supply that begins in 2008.
The development combines Altairnano’s proprietary nanometal oxide dispersion technology and PPG’s proprietary resin to create a primer that will replace today’s chromate-based coatings, according to Paul Bowman, PPG Aerospace global business platform manager for coatings.
Under the agreements, Altairnano will make the nanometal oxide chemical dispersion using PPG’s proprietary resin technology to meet the final paint requirements.
“The technology will be developed for primer in both interior structural and exterior fuselage applications, giving customers a safe, sound solution to eliminate chromate from the production stream,” Bowman said. “It represents the first time we will be able to have a primer that works similarly to chromate-containing materials without the environmental issues involved in the use of chromates.”
Bowman said the technology also looks promising for the creation of other corrosion-resistant coatings, and the companies expect to commercialize the chromate-free primer later this year.
Altair Nanotechnologies Chief Executive Officer Alan Gotcher, Ph.D., said, “We are enthusiastic to be working with the world’s largest aerospace coatings company to develop, commercialize and manufacture this green technology.”
For more information, visit http://corporate.ppg.com/ppg/aerospace/default.htm.
PPG Industries’ aerospace business and Altair Nanotechnologies have agreed to jointly develop and commercialize environmentally friendly nanoparticle technology to replace chromate in an aircraft primer that affords excellent corrosion resistance in high-solids and waterborne formulas. Terms were not disclosed.
The companies will develop a nanometal oxide dispersion technology under a three-year research agreement, with an added five-year contract for commercialization and supply that begins in 2008.
The development combines Altairnano’s proprietary nanometal oxide dispersion technology and PPG’s proprietary resin to create a primer that will replace today’s chromate-based coatings, according to Paul Bowman, PPG Aerospace global business platform manager for coatings.
Under the agreements, Altairnano will make the nanometal oxide chemical dispersion using PPG’s proprietary resin technology to meet the final paint requirements.
“The technology will be developed for primer in both interior structural and exterior fuselage applications, giving customers a safe, sound solution to eliminate chromate from the production stream,” Bowman said. “It represents the first time we will be able to have a primer that works similarly to chromate-containing materials without the environmental issues involved in the use of chromates.”
Bowman said the technology also looks promising for the creation of other corrosion-resistant coatings, and the companies expect to commercialize the chromate-free primer later this year.
Altair Nanotechnologies Chief Executive Officer Alan Gotcher, Ph.D., said, “We are enthusiastic to be working with the world’s largest aerospace coatings company to develop, commercialize and manufacture this green technology.”
For more information, visit http://corporate.ppg.com/ppg/aerospace/default.htm.