The ISO-Automat P2 from ELMED is designed to test diverse kinds of coatings reliably. According to the company, even the smallest pores and faults are detected dependably and without damaging the material.

The flexibility of the complete turnkey system allows adaptation to international test standards, specific coating processes such as side extrusion and crosshead extrusion, and semi- and fully automatic testing.

The integrated, network-compatible industrial PC monitors and documents the parameters of the modular test system. A contact-free color marking system is supported by a pipe end detection and tracking system and simplifies the discovery of faults by closely marking the positions of pores.

For more information, visit www.isotest.de.