Cytec Launches Waterborne UV Curable Resin - Posted 3/27/07

March 27, 2007
UCECOATĀ® 7631 waterborne UV curable resin from Cytec Industries Inc. is designed for use in topcoats on outdoor wood joinery. The aliphatic polyurethane dispersion reportedly offers superior weathering resistance, as well as outstanding chemical and mechanical resistance.

UCECOATĀ® 7631 waterborne UV curable resin from Cytec Industries Inc. is designed for use in topcoats on outdoor wood joinery. The aliphatic polyurethane dispersion reportedly offers superior weathering resistance, as well as outstanding chemical and mechanical resistance.

According to the company, the translucent dispersion is non-irritant (Xi-free), low-VOC, and has good colloidal stability. It can be easily formulated and applied by either spray or curtain coating in safe conditions. Other features include high flexibility and tack-free properties after water evaporation.

For more information, call 800.652.6013 or 973.357.3193, e-mail custinfo@cytec.com or visit www.cytec.com.