Arkema to Increase Kynar® Production Capacity (7/25/06)

July 25, 2006

Arkema, a manufacturer of the high performance technical polymer polyvinylidene fluoride (PVDF) distributed under the tradename Kynar, intends to increase its production capacity at its Calvert City, KY facility by more than 2,000 tons a year. The investment is expected to be $12 million.

Scheduled for completion in early 2008, this capacity increase will make Kynar unit production in Calvert City one of the largest PVDF plant in the world, strategically placed to supply both American and Asian markets. Like Arkema's PVDF plant in Pierre-Benite, France, the Calvert City plant benefits from integrated monomer feedstocks, efficient technology, and experienced manufacturing personnel.