COATING 2005 EXHIBITORS HIGHLIGHTS: Paint Stripping Processes

August 1, 2005
Recover is for reclaiming defectively coated parts and components. Effective on most organic coatings, including e-coat, powders and multilayer liquid paints, Recover processes are designed to offer performance and versatility. Processes can be used on ferrous alloys (including galvanized steels), pot metals, aluminum, copper, brass, and select resins such as nylon and TPO.

Kolene Corp.

800-521-4182; www.kolene.com

Booth 1610