Researchers Reveal Nano-Properties of Eucalyptus
November 4, 2011
PERTH, Australia - Murdoch University nano scientists have discovered that a eucalyptus plant native to south west Western Australia has unique self-cleaning and water-repellent properties that could make it a gold mine for new nanotechnology applications.
The Mottlecah, which is also known as The Rose of the West for its large spectacular flowers, has silvery leaves that are covered in a wax that produces nano-sized bumps and pillars. This causes water to form droplets that roll over the surface of the leaves and fall towards the root system of the plant, picking up any dirt along the way.
These properties, known as superhydrophobic and self-cleaning, are similar to those of the lotus plant, which has inspired a range of self-cleaning and anti-bacterial technologies currently being developed.
Dr. Gerrard Eddy Jai Poinern and his team at the Murdoch Applied Nanotechnology Research Group say their discovery has the potential to be applied in a variety of ways, from so-called lab-on-a-chip settings in medical research, to the treatment of ships’ hulls to help prevent the buildup of harmful microorganisms, plants, and animals.
“I had noticed these incredible plants on the Murdoch campus because of the unusual appearance of their leaves,” said Poinern, who is based at the School of Engineering and Energy. “They made me wonder whether the plant had superhydrophobic properties and so began our research investigation.
“One of the experiments we carried out was to coat the leaf with carbon black toner from a laser printer cartridge and then observe how the rolling drops of water were able to completely clean the surface of the leaf.
“This was because the surface features formed by this eucalyptus’ waxes gave the leaves remarkable wetting and self-cleaning properties. We believe this enhances the plant’s survival in an arid climate, because it is able to source and effectively manage its water usage through channeling any water to its roots. In this way, the Mottlecah is unusual because most superhydrophobic plants are usually found in aquatic settings.”
Poinern and his team also extracted waxes from the leaves and found that they were capable of self-reassembly. When coated on laboratory glass slides, the wax formed features that mimicked the complex three-dimensional geometry of the nano-sized bumps and pillars found on the original leaf surface, making the slide superhydrophobic.
“It was fairly easy and inexpensive to extract the wax from the leaves, and yet the wax still had these remarkable qualities,” said Poinern. “When the tested glass slides were placed horizontally onto a water surface, the added buoyancy support of the wax meant that it was able to carry a greater load than the uncoated slides. In microfluidic devices used in advanced medical research and disease testing, such coatings could help to maintain the sterility of devices which need to be used over and over again. In fact, there are a number of potential applications, and we are sure there are other WA native plants which have similar properties. We hope to continue our research to find out more about these properties and how they can be fully utilized.”
Recognized as one of Australia’s leading research institutions, Murdoch University, Perth, Australia, has over 18,000 students enrolled in over 200 undergraduate and postgraduate courses across a wide range of disciplines.
The Mottlecah, which is also known as The Rose of the West for its large spectacular flowers, has silvery leaves that are covered in a wax that produces nano-sized bumps and pillars. This causes water to form droplets that roll over the surface of the leaves and fall towards the root system of the plant, picking up any dirt along the way.
These properties, known as superhydrophobic and self-cleaning, are similar to those of the lotus plant, which has inspired a range of self-cleaning and anti-bacterial technologies currently being developed.
Dr. Gerrard Eddy Jai Poinern and his team at the Murdoch Applied Nanotechnology Research Group say their discovery has the potential to be applied in a variety of ways, from so-called lab-on-a-chip settings in medical research, to the treatment of ships’ hulls to help prevent the buildup of harmful microorganisms, plants, and animals.
“I had noticed these incredible plants on the Murdoch campus because of the unusual appearance of their leaves,” said Poinern, who is based at the School of Engineering and Energy. “They made me wonder whether the plant had superhydrophobic properties and so began our research investigation.
“One of the experiments we carried out was to coat the leaf with carbon black toner from a laser printer cartridge and then observe how the rolling drops of water were able to completely clean the surface of the leaf.
“This was because the surface features formed by this eucalyptus’ waxes gave the leaves remarkable wetting and self-cleaning properties. We believe this enhances the plant’s survival in an arid climate, because it is able to source and effectively manage its water usage through channeling any water to its roots. In this way, the Mottlecah is unusual because most superhydrophobic plants are usually found in aquatic settings.”
Poinern and his team also extracted waxes from the leaves and found that they were capable of self-reassembly. When coated on laboratory glass slides, the wax formed features that mimicked the complex three-dimensional geometry of the nano-sized bumps and pillars found on the original leaf surface, making the slide superhydrophobic.
“It was fairly easy and inexpensive to extract the wax from the leaves, and yet the wax still had these remarkable qualities,” said Poinern. “When the tested glass slides were placed horizontally onto a water surface, the added buoyancy support of the wax meant that it was able to carry a greater load than the uncoated slides. In microfluidic devices used in advanced medical research and disease testing, such coatings could help to maintain the sterility of devices which need to be used over and over again. In fact, there are a number of potential applications, and we are sure there are other WA native plants which have similar properties. We hope to continue our research to find out more about these properties and how they can be fully utilized.”