AkzoNobel Forms Partnership to Secure TiO2 Supply

August 1, 2011

AMSTERDAM, the Netherlands – AkzoNobel has entered into a partnership in China with Quangxi CAVA Titanium Industry Co. Ltd. for the production and supply of titanium dioxide (TiO2). The collaboration includes the construction of a new TiO2 plant in Qinzhou, China.