www.pcimag.com/articles/92914-akzonobel-coatings-protect-oakland-bay-bridge
AkzoNobel Coatings Protect Oakland Bay Bridge
August 17, 2011
AMSTERDAM, the Netherlands - Coatings supplied by International Paint will ensure lasting protection for the east span of the San Francisco-Oakland Bay Bridge. The east span had to be rebuilt after being damaged by the Lorna Prieta earthquake in 1989.
International Paint was selected as the sole coatings supplier for the project by Shanghai Zhenhua Heavy Industry Group Ltd. (ZPMC), which supplied the steel structures for the east span rebuild. The sections were coated in China and shipped to the United States for installation.
The project used a total of 500,000 liters of International® coatings, including inorganic zinc-rich primer Interzinc® 22, which provides long-term corrosion resistance; and Interfine® 979 acrylic polysiloxane finish, which gives excellent color and gloss retention. The coatings were manufactured at International Paint’s factory in Suzhou and come with a 20-year warranty.
ZPMC is a leading equipment manufacturing company. Its main products include large-scale container machinery and bulk cargo handing machinery, offshore heavy-duty products, heavy-duty steel structures, energy-conservative and environment-friendly equipment and accessories.
International Paint was selected as the sole coatings supplier for the project by Shanghai Zhenhua Heavy Industry Group Ltd. (ZPMC), which supplied the steel structures for the east span rebuild. The sections were coated in China and shipped to the United States for installation.
The project used a total of 500,000 liters of International® coatings, including inorganic zinc-rich primer Interzinc® 22, which provides long-term corrosion resistance; and Interfine® 979 acrylic polysiloxane finish, which gives excellent color and gloss retention. The coatings were manufactured at International Paint’s factory in Suzhou and come with a 20-year warranty.
ZPMC is a leading equipment manufacturing company. Its main products include large-scale container machinery and bulk cargo handing machinery, offshore heavy-duty products, heavy-duty steel structures, energy-conservative and environment-friendly equipment and accessories.