According to the latest research data from China Chemicals Market, a Chinese consulting company based in Guangzhou, China, the total capacity of China’s titanium dioxide (TiO2) represents approximately 30 percent of world capacity.
GUANGZHOU, China – According to the latest research data from China Chemicals Market, a Chinese consulting company based in Guangzhou, China, the total capacity of China’s titanium dioxide (TiO2) represents approximately 30 percent of world capacity. In 2010, the total capacity of China’s TiO2 reached 2,000,000 tonnes, and annual production reached 1,470,000 tonnes.
According to the study, China has become the largest consumer of TiO2 in the world. In 2010, the consumption of TiO2 in China exceeded 1,400,000 tonnes. Demand for TiO2 is expected to grow at about 10 percent annually in the coming years.
For additional information about this study, visit www.cnchemicals.com.
GUANGZHOU, China – According to the latest research data from China Chemicals Market, a Chinese consulting company based in Guangzhou, China, the total capacity of China’s titanium dioxide (TiO2) represents approximately 30 percent of world capacity. In 2010, the total capacity of China’s TiO2 reached 2,000,000 tonnes, and annual production reached 1,470,000 tonnes.
According to the study, China has become the largest consumer of TiO2 in the world. In 2010, the consumption of TiO2 in China exceeded 1,400,000 tonnes. Demand for TiO2 is expected to grow at about 10 percent annually in the coming years.