www.pcimag.com/articles/91862-patent-awarded-for-innovative-see-cure-technology
Patent Awarded for Innovative See-Cure Technology
March 1, 2011
DYMAX Corporation has been issued a patent covering the invention of its See-Cure color-change technology.

DYMAX Corporation, an ISO 9001-certified manufacturer of advanced light-curable materials and light-curing systems, has been issued U.S. Patent number 7,691,557, Polymerizable Composition Exhibiting Permanent Color Change as Cure Indicator, covering the invention of its See-Cure color-change technology. This technology, developed by Dr. Stephen Cantor and Dr. Igor Khudyakov, addresses the two most-often asked questions about light-curable products: “How do I know I have dispensed enough adhesive?” and “How do I know when the adhesive is cured?”
DYMAX adhesives formulated with See-Cure technology are bright blue in color in their uncured state, making them very easy to see on the surface of substrates, in deep wells, or when sandwiched between two layers of transparent or translucent material. Because the blue color is extremely visible, simple vision systems can be incorporated into assembly processes prior to curing in order to easily identify adhesive coverage and profile.
The blue color in See-Cure adhesive technology is only temporary. The disappearance of the adhesive’s blue color is the visible indicator that sufficient light energy has been provided to achieve full cure. As the adhesive cures, the blue color fades and the adhesive ultimately turns clear upon full cure.
In addition to their headquarters in Torrington, DYMAX has locations in Germany, China, Hong Kong, and Korea which serve the assembly needs of the medical, electronic, optical, automotive, appliance, metal finishing, power generation, and industrial markets worldwide.
DYMAX Corporation is a leading technology-based company specializing in the formulation, manufacture, and service of advanced assembly adhesives, coatings, epoxies, masking resins, and light-curing systems.
For more information, e-mail info@dymax.com or visit www.dymax.com.

DYMAX Corporation, an ISO 9001-certified manufacturer of advanced light-curable materials and light-curing systems, has been issued U.S. Patent number 7,691,557, Polymerizable Composition Exhibiting Permanent Color Change as Cure Indicator, covering the invention of its See-Cure color-change technology. This technology, developed by Dr. Stephen Cantor and Dr. Igor Khudyakov, addresses the two most-often asked questions about light-curable products: “How do I know I have dispensed enough adhesive?” and “How do I know when the adhesive is cured?”
DYMAX adhesives formulated with See-Cure technology are bright blue in color in their uncured state, making them very easy to see on the surface of substrates, in deep wells, or when sandwiched between two layers of transparent or translucent material. Because the blue color is extremely visible, simple vision systems can be incorporated into assembly processes prior to curing in order to easily identify adhesive coverage and profile.
The blue color in See-Cure adhesive technology is only temporary. The disappearance of the adhesive’s blue color is the visible indicator that sufficient light energy has been provided to achieve full cure. As the adhesive cures, the blue color fades and the adhesive ultimately turns clear upon full cure.
In addition to their headquarters in Torrington, DYMAX has locations in Germany, China, Hong Kong, and Korea which serve the assembly needs of the medical, electronic, optical, automotive, appliance, metal finishing, power generation, and industrial markets worldwide.
DYMAX Corporation is a leading technology-based company specializing in the formulation, manufacture, and service of advanced assembly adhesives, coatings, epoxies, masking resins, and light-curing systems.