www.pcimag.com/articles/91336-astm-committee-approves-new-lead-paint-standard

ASTM Committee Approves New Lead Paint Standard

August 15, 2010

WASHINGTON, D.C. - A new ASTM International standard will provide the means to quickly detect and quantify the lead concentration in toys and other children's products. The new standard, F2853, Test Method for Determination of Lead in Paint Layers and Similar Coatings or in Substrates and Homogenous Materials by Energy Dispersive X-Ray Fluorescence Spectrometry Using Multiple Monochromatic Excitation Beams, was developed by Subcommittee F40.01 on Test Methods, part of ASTM International Committee F40 on Declarable Substances in Materials. The analytical technique described in this standard is commonly referred to as HDXRF.

“Frequent testing of children's products aids in identifying sources of lead contamination and ultimately prevents out-of-compliance merchandise from reaching store shelves,” said Berry Beumer, Vice President, XOS Inc., and Chairman of the task group that developed F2853.

ASTM F2853 provides a convenient means to test for lead using the energy dispersive X-ray fluorescence spectroscopy technique. Such testing will ensure that toys and other children's products will comply with laws (such as the Consumer Product Safety Improvement Act of 2008) that are currently being enforced by the U.S. Consumer Product Safety Commission.

According to Beumer, the HDXRF test described in F2853 enables lead quantification separately for the substrate and paint level in a five-minute measurement cycle. Beumer notes that all interested parties are invited to join the task group responsible for F2853 as it considers future revisions to the standard.