www.pcimag.com/articles/90705-malvern-instruments-offers-new-elearning-course
Malvern Instruments Offers New eLearning Course
May 21, 2010
Malvern Instruments has introduced a comprehensive eLearning course that details light scattering for materials characterization using the company’s Zetasizer Nano system.
MALVERN, UK - Malvern Instruments has introduced a comprehensive eLearning course that details light scattering for materials characterization using the company’s Zetasizer Nano system. Course modules introduce dynamic and electrophoretic light-scattering techniques as well as sample preparation, instrument configuration and how to set up standard operating procedures.
Two course admissions are being offered free of charge with every Zetasizer Nano purchased. For additional information, visit www.malvern.com/elearning.