CHICAGO - Ravin Gandhi and Kanti Gandhi, former owners of Coatings and Chemicals Corp. (CCC), have returned to the non-stick coatings industry with a joint venture coatings company called GMM Development Limited.

The new company is based in Zhuhai, China, and employs 200 people in four different divisions, including a coatings manufacturing plant, a research and development lab, a sales and technical service team, and a coatings spraying factory.