www.pcimag.com/articles/87786-smart-adhesive

Smart Adhesive

May 5, 2008
In this demonstration of gecko-inspired adhesive, increasing the supported weight increases the contact area (bright area near top of patch). The adhesive is “smart”’ in that a greater load causes more microfibers to engage, increasing adhesion strength. Decreasing the load allows the fibers to disconnect, making release easy. (Photos by Jongho Lee/UC Berkeley.)

A new anti-sliding adhesive developed by engineers at the University of California, Berkeley, may be the closest man-made material yet to mimic the remarkable gecko toe hairs that allow the tiny lizard to scamper along vertical surfaces and ceilings.

The researchers say that such an adhesive could one day be used to outfit a small robot that could climb up walls.

Taking a cue from the millions of hairs covering a gecko’s toes, researchers squeezed 42 million hard plastic microfibers onto each square centimeter of material and loaded it with various weights. They found that on a smooth, clean, vertical surface, two square centimeters of the synthetic adhesive could hold 400 grams (0.88 pounds). At the same time, the adhesive easily lifts off with minimal force and no residue.

Scientists have long marveled at the gravity-defying feats of the gecko, and a number of research teams across the world are working on duplicating the lizard’s adhesive forces. Ron Fearing, UC Berkeley professor of electrical engineering and computer sciences and head of the research team developing the new material, notes that previous research on gecko-like adhesives has focused on the strength of the adhesion. He said that the ease of attachment and detachment are equally important when developing a material that can practically be used for scaling vertical walls and ceilings.

What sets this new gecko-inspired adhesive apart from the others created thus far is that it is directional, only “sticking” when it slides along a smooth surface, not when it is pressed down.

“This difference is critical because if you’re climbing up vertical surfaces, you can’t afford to use a lot of energy pressing down into the surface to stick,” said Fearing. “Using force to attach also requires force to detach. A gecko running uphill may be attaching and detaching its feet 20 times a second, so it’d get very tired if it had to work hard to pull its feet off at every step.”

The microfibers, made of polypropylene, are 20 microns long, or one-fifth the thickness of a sheet of paper, with a diameter of 0.6 microns, or one-hundredth the diameter of a human hair.

The structure is similar to a microfiber array developed by the same group in 2006. That material relied upon friction to work, however, requiring the application of force to make it stick. Changes made to the plastic backing enabled the directional adhesion reported in this new material to work on truly vertical surfaces.

“For a gecko, this seemingly subtle change could mean the difference between life or death,” said Fearing. “With friction only, a gecko would fall from a wall or ceiling. With directional adhesion, a gecko can stop itself from falling because the mechanism works without the need for force that is perpendicular to the surface.”

The new research is described in a pair of papers published online Jan. 23 in the Journal of the Royal Society Interface. Members of Fearing’s UC Berkeley research team are Jongho Lee, a graduate student in mechanical engineering, and Bryan Schubert, a graduate student in electrical engineering and computer sciences. Co-author Carmel Majidi, a former UC Berkeley graduate student in electrical engineering and computer sciences, is now a post-doctoral researcher at Princeton University.

Side view of polypropylene microfiber array.

“This is a major milestone in the new field of gecko-inspired adhesives,” said Kellar Autumn, associate professor of biology at Lewis & Clark College in Portland, Ore., who is considered one of the nation’s leading experts on gecko movement and who was not a co-author on this latest research. “Fearing’s like-real-gecko-protein-adhesive is made from a plastic that is very hard; it is not sticky to the touch. Also, just like what we found in real gecko foot hairs, Fearing’s microfiber arrays are sticky only when they slide across a surface. This could be the first real gecko tape.”

Fearing and his colleagues are part of a Nanoscale Interdisciplinary Research Team supported by the National Science Foundation and specifically tasked in 2003 with developing synthetic adhesives that perform like gecko hairs.

In 2000, Fearing teamed up with biologists Robert Full at UC Berkeley and Autumn at Lewis & Clark, and engineer Thomas Kenny from Stanford University, in the first study pointing to the secret of gecko adhesion: intermolecular van der Waals forces that remain weak until surfaces get intimately close. Two years later, members of this same team synthesized gecko hair tips that stick, providing the first direct experimental verification of a van der Waals mechanism for gecko foot-hair adhesion.

Not only is each gecko toe covered by millions of tiny hairs, but those hairs are further split at the end into billions of nanoscale spatulae. The van der Waals forces come into play when these spatulae make contact with the surface.

This new material is also an example of a “smart adhesive,” becoming stronger with use, said Fearing, who is also part of UC Berkeley’s Center for Information Technology Research in the Interest of Society. “More microfibers bend and engage automatically as the weight increases. When the load is removed, the microfibers disengage. This allows for controlled attachment and detachment and is a critical innovation for clean release and reuse. It’s the first time this has been demonstrated with a hard microfiber array.”

Another benefit to using hard polymers is that the fibers are less prone than softer plastic to collecting dirt after repeated use. So far, the new adhesive only works on smooth, clean surfaces. The next step, said Fearing, is to develop a material that can also adhere to rough surfaces and that is self-cleaning.