www.pcimag.com/articles/87705-basf-increases-acrylic-monomers-prices-in-north-america

BASF Increases Acrylic Monomers Prices in North America

June 9, 2008

Effective June 1, 2008, or as contracts allow, BASF will increase its prices on its acrylic monomers sold in the United States, Canada and Mexico. Glacial acrylic acid will increase $0.04 per pound. Methyl acrylate will increase $0.05 per pound. Ethyl acrylate will increase $0.05 per pound. Butyl acrylate will increase 0.05 per pound, and 2-ethylhexyl acrylate will increase 0.07 per pound.