www.pcimag.com/articles/87441-thermo-fisher-scientific-announces-an-agreement-to-distribute-ebsd-systems
Thermo Fisher Scientific Announces an Agreement to Distribute EBSD Systems
November 1, 2007

MADISON, WI - Thermo Fisher Scientific Inc. has signed an agreement with Edax, a business unit of the Ametek Materials Analysis Division, to distribute its Electron Backscatter Diffraction (EBSD) Systems. Featuring Edax’s advanced Orientation Imaging Microscopy technology (OIM™), the EBSD system will add unique capabilities to Thermo Fisher’s existing microanalysis offering. OIM is an advanced EBSD system available for analyzing crystal orientations in a sample.